Dissolving Agent
Dissolving Agent
Dissolving Agent
  • Dissolving Agent

General Introduction of Dissolving Agent

It is a compound smetling flux for magnesium and its alloy, to protect magnesium melt and accelerate the melting rate.

Function of Dissolving Agent

The combination of magnesium and potassium chlorides provides the low melting eutectic,while the fluoride provides the surface wettability and chemical reactivity with magnesium oxide to cause sufficient removal. MgO increases the viscosity of flux. The barium compound provides the density requirement for the salt to effectively mix with the magnesium and then settle out at the bottom of the crucible.

flux

Main composition(%)

MgCl2

KCl

BaCl2

CaF2

NaCl

CaCl2

MgO

Insoluable Substance

H2O

Dissolving Flux

42-48

33-37

5-9

--

8-12

<1.5

---

≤1.5

≤1.5




See More
  • Granulated Calcium Removal Flux

    Granulated Calcium Removal Flux

    October 13, 2021General Description of Granulated Calcium Removal FluxCalcium is a kind of impurity in aluminium alloys; Ca reacts with Aluminium alloy to form the CaAl4 compound which will destroy the surface’s fil...view
  • Mg Ingot

    Mg Ingot

    December 25, 2020General DescriptionMagnesium metal is a new type of lightweight and corrosion-resistant metal material. It is a silver-white metallic luster.Function: 1.It has superior properties such as low specific...view
  • Magnesium Chloride Hexahydrate Flake

    Magnesium Chloride Hexahydrate Flake

    September 18, 2019Magnesium Chloride Hexahydrate FlakeGeneral Description of Magnesium Chloride Hexahydrate FlakeChemically, magnesium chloride is represented as MgCl2. It is a naturally occurring mineral salt which is...view
  • Furnace Cleaning Flux

    Furnace Cleaning Flux

    September 6, 2019Furnace Cleaning Flux (SATA-PF-390)Description of Furnace Cleaning Flux (SATA-PF-390)Slag will be generated in the furnace during smelting after a period of time, which not only shorten the life of re...view
Leave a Message Email Us

we will contact you within 24 hours.